Notice: Function _load_textdomain_just_in_time was called incorrectly. Translation loading for the wordpress-seo domain was triggered too early. This is usually an indicator for some code in the plugin or theme running too early. Translations should be loaded at the init action or later. Please see Debugging in WordPress for more information. (This message was added in version 6.7.0.) in /var/www/html/wp-includes/functions.php on line 6260 Professional Relaxer - Happi

Professional Relaxer

Professional Relaxer
Ingredients
%

Phase A

  • Deionized water
  • 51.90
  • Propylene glycol
  • 2.00
  • Syntran PC 5208 (Polyacrylate-15)
  • 8.00

Phase B

  • Polawax NF (Croda) (Emulsifying wax NF)
  • 7.50
  • Cetyl alcohol (Protameen)
  • 1.00
  • Snow White petrolatum (Penreco) (Petrolatum)
  • 8.00
  • Drakeol 7 Lt. mineral oil (Penreco) (Mineral oil)
  • 11.00
  • Volpo 10 (Croda) (Oleth-10)
  • 2.00
  • Brij 72 (Uniqema) (Steareth-2)
  • 0.50

Phase C

  • Deionized water
  • 6.00
  • Sodium hydroxide
  • 2.10

Procedure

Add water, propylene glycol and Syntran PC 5208 to vessel and begin heating to 75-80°C. Stir until batch is homogenous. With batch at 75-80°C, individually add each Phase B ingredient to batch. Stir between each addition until homogenous emulsion results. Cool batch to 35°C. In a separate water cooled vessel with high shear stirring prepare Phase C. Caution: Premix will become extremely hot, cool as needed. Slowly add Phase C to batch. Homomix until batch is homogenous and smooth. Appearance: Low viscosity, glossy, white creme. pH = 12.6-12.9.